Stress relieve at 1050 deg F for 1 hr; heat at 1500/1550 deg F; quench in salt at 700 deg F; hold 45 min, air cool; reheat; oil quench; temper 1 hr; finish: 125 micro inches; harden to Rockwell C51-C59; ctr hole 0.375 in. dia located 4.340 in. from 1st end; matl-steel or steel ASTM A331; surface treat. phosphate manganese or phosphate zinc
Material (MATT)
Steel
Surface Treatment (SFTT)
Phosphate
Catalogue data is compiled from public DLA/FLIS sources and is provided for
identification. Availability, condition and certification are confirmed on
quotation. OmniSynk Distribution Services is a stocking distributor.